Cell would be heated up during formation, which improve the fluidity of electrolyte, strengthen the viscosity of electrolyte, with homogeneously spread of electrolyte, SEI would be formed easily, cycle life could be extended; Cooling compression could cool down the cell temperature quickly, under this format cell would be in good performance, low bulge rate and long cycle life, etc.